Pad Printing Problems

Pad Print
Process FAQs

PAD PRINT PROCESS PROBLEMS - FAQs:

(Click on a Question to view the Answer)

1. There is a light spot in my print. How do I fix this?
2. The ink is not picked from the plate. What should I do?
3. Why can't I get full release of the image from the pad?
4. I'm getting small holes in my print. What's causing it?
5. Why do my plates wear out fast / scratch easily?
6. What's the most common plate problem?
7. Why does my image look fuzzy, with "spider webs" in it?
8. My image is not opaque enough. How can I make it better?
9. The image is distorted at the edges. What should I do?
10. Why am I getting inconsistent image placement on my part?
11. Previously cured prints became sticky after a few days. Why?
12. Ink becomes thick too quickly. What's causing it?
13. How do I know whether ink viscosity is correct, whether it has enough thinner?
14. My print starts to disappear after 5-10 parts are run. I stop the machine for a period of time, then start again - and the print comes back. Why?



Answers:

1. There is a light spot in my print. How do I fix this?
Most likely reasons:
- The light spot may be caused by plate scooping. If so, use a lower line screen (approximately 150 lines per inch).
- The spot can also be created by the point of the pad. In this case, select a pad with a lower point.



2. The ink is not picked from the plate. What should I do?
The ink is most likely drying in the etch. Make sure that:
- Plates are not too shallow.
- Ink is not too fast.
- Pad is not old/worn out.
- Ink cup has sufficient ink.



3. Why can't I get full release of the image from the pad?
It is most likely one of the following two reasons: a) the ink is either too wet or too dry or b) the pad is old.

a) To determine if it is an ink problem, touch the pad immediately after ink pick up. If the ink does not transfer to your hand, it is too dry. It means that your plate is too shallow or the thinner is too fast. If the ink does transfer, it may be too wet. Make sure your plate is not too deep and thinner is not too slow.

b) To determine if the pad has dried out see if it just will not release ink no matter the ink formulation. The pad will not release ink if it has dried out. Depending on the degree of dryness, you need to replace the pad or restore it. Try our Nu-Pad Conditioner & Restorer formulated to replenish pad oils.    Request a sample



4. I'm getting small holes in my print. What's causing it?
What typically causes "pinholes" is air being trapped in the etch by the pad. Possible reasons:
- Pad is too soft or too flat. Try a harder and pointier one.
- Plate is too deep. Try a shallower plate.



5. Why do my plates wear out fast / scratch easily?
Possible reasons:
- Plates have not been fully post-cured. If you are able to dig your fingernail into the plate, you should post cure it for a longer period of time. Hint: leaving your plate in direct sunlight will post cure faster than most exposure systems.
- The pressure on the cup is too high.
- There is not enough ink in the ink cup causing the plate not to be lubricated. We recommend no less than 40 grams of ink in a 90mm cup.



6. What's the most common plate problem?
- A plate being too shallow, which causes the ink to dry too fast. Please note: the shorter the exposure, the deeper you want the plate!



7. Why does my image look fuzzy, with "spider webs" in it?
Possible causes:
- Plate is too deep.
- There is static electricity. Antistatic paste or Antistatic liquid for inks will resolve this problem.    Request samples
- Ink is too thick.
- Pad is too flat.



8. My image is not opaque enough. How can I make it better?
- Check to make sure the pad is not overcompressing.
- Make sure plate is not too shallow.
- Make sure ink is not too thin.
- Use a harder pad which will pick up and lay down more ink.
- Try high density ink.



9. The image is distorted at the edges. What should I do?
It's a pad selection problem. If possible, use a larger pad (20% increase will most likely fix it). Alternatively, use a softer pad.



10. Why am I getting inconsistent image placement on my part?
- Possible causes:
- Part is not fixed properly and is "rocking."
- Plate is not secured on the machine.
- Pad mount in not secured.
- Pad is too soft.



11. Previously cured prints became sticky after a few days. Why?
Rewetting is caused by plasticizers that migrate from the part to the ink. This is common for vinyl. You need to use ink designed specifically for vinyl.    Request free adhesion test



12. Ink becomes thick too quickly. What's causing it?
Possible reasons:
- There is too much hardener.
- THhere is not enough thinner or wrong type of thinner.
- Ink is contaminated at mixing. Make sure your mixing container and mixing sticks as well as cleaners are acetone- and plasticizer-free. Contact ICN to consult!



13. How do I know whether ink viscosity is correct, whether it has enough thinner?
- In general, we recommend weighing ink and thinner when mixing. Typically the mixture is 15% thinner to the weight of the ink.
- To test mixed ink viscosity: dip a mixing stick, pull it out and allow the ink to drip from the stick, forming a figure 8 (the size that would fit in 8 ounce drinking cup). If the 8 disappears before you finish it, the ink is too thin. If ink puddles on top or if the 8 does not start disappearing by the time you finish it, the ink is too thick.



14. My print starts to disappear after 5-10 parts are run. I stop the machine for a period of time, then start again and the print comes back. Why?

- Thinner is too fast. Speed up the machine or mix new ink with slower thinner or retarder.
- The plate is too shallow and the ink is drying out.




 
Team Inkcups Local Sales & Tech Support
We have direct sales people in the US (MA, NY, CA, IA, GA), Canada, Mexico, Guatemala, Honduras. We also have respresentatives in Colombia and Dominican Republic.

Contact Inkcups!
Tagless pad printing Apparel Tag Printing!

Turnkey solution for tagless t-shirt printing: complete line of Equipment & Supplies, plus unlimited tech support!

Read more